性能項目 | 測試條件 | 測試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | 185/115 | kg/cm2(MPa)[Lb/in2] | |
斷裂伸長率 | ASTM D638/ISO 527 | % | |||
拉伸模量 | ASTM D638/ISO 527 | 9500/6200 | kg/cm2(MPa)[Lb/in2] | ||
拉伸屈服伸長率(延伸率) | ASTM D638/ISO 527 | % | |||
拉伸斷裂伸長率(延伸率) | ASTM D638/ISO 527 | % | |||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 8600/5000 | kg/cm2(MPa)[Lb/in2] | ||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | 270/190 | kg/cm2(MPa)[Lb/in2] | ||
洛氏硬度 | ASTM D785 | ||||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | 95/110 | kg·cm/cm(J/M)ft·lb/in | |
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(無缺口) | ASTM D256/ISO 179 | 15/30 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(無缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1360 | ||
成型收縮率 | ASTM D955 | % | |||
熔融指數(shù)(流動系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | g/10min | ||
220℃/10kg | ASTM D1238/ISO 1133 | g/10min | |||
吸水率 23℃/24H | ASTM D570/ISO 62 | % | |||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | ℃(℉) | |
未退火 | ASTM D648/ISO 75 | 210 | ℃(℉) | ||
維卡軟化點(diǎn) | ASTM D1525/ISO R306 | ℃(℉) | |||
熔點(diǎn) | - | ℃(℉) | |||
燃燒性(率) | UL94 | ||||
線性膨脹系數(shù) | ASTM D696/ISO 11359 | 2-2.5/6-7 | mm/mm.℃ | ||
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 | 3.8/6.8 | |
1MHZ | ASTM D150/IEC 60250 | ||||
體積電阻率 | ASTM D257/IEC 60093 | 10/10 | Ω.cm | ||
表面電阻率 | ASTM D257/IEC 60093 | 10/10 | Ω | ||
耐電弧性 | ASTM D495/IEC 60112 | ||||
加工條件 | 干燥條件 | ||||
加工溫度 | 射嘴 | ℃ | |||
料筒前段 | ℃ | ||||
料筒中段 | ℃ | ||||
料筒后段 | ℃ | ||||
熔體溫度 | ℃ | ||||
模具溫度 | ℃ | ||||
壓力 | 注塑壓力 | Mpa | |||
保壓壓力 | Mpa | ||||
背壓 | Mpa | ||||
螺桿轉(zhuǎn)速 | rpm | ||||
其他 | 備注 | ||||
顏色 | |||||
特性 | 注塑級,玻纖增強(qiáng),用于需要高剛性和尺寸穩(wěn)定性,耐熱老化的部件 |
PA6/德國巴斯夫/B3EG6 增強(qiáng)級 耐老化性