PC IRY2200 日本出光石油化學(xué)株式會(huì)社 物性數(shù)據(jù) |
①原料描述部分
規(guī)格級(jí)別: | 阻燃級(jí) | 外觀顏色: | --- |
用途概述: | --- | ||
備注說明: | 特性:低粘度、防火等級(jí)新V-0 |
②原料技術(shù)數(shù)據(jù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 吸水率 | --- | --- | 0.23 | % |
熔體流動(dòng)速率 | --- | --- | 12 | g/10min | |
物理性能 | 光線透射率 | --- | --- | 85~89 | % |
比重 | --- | --- | 1.20 | --- | |
機(jī)械性能 | 伸張屈服強(qiáng)度 | --- | --- | 64 | MPa |
伸張抗斷強(qiáng)度 | --- | --- | 68 | MPa | |
伸張彈性模量 | --- | --- | 2300 | MPa | |
破壞伸張率 | --- | --- | 115 | % | |
抗撓強(qiáng)度 | --- | --- | 93 | MPa | |
彎曲彈性模量 | --- | --- | 2350 | MPa | |
IZOD沖擊強(qiáng)度 | 4mm | --- | 70 | KJ/m2 | |
IZOD沖擊強(qiáng)度 | 3.2mm | --- | 90 | KJ/m2 | |
羅氏硬度 | --- | --- | R120(M75) | --- | |
滑動(dòng)摩擦 | --- | --- | 12 | --- | |
電氣性能 | 絕緣破壞電壓 | --- | --- | 30 | kv/mm |
體積固有電阻 | --- | --- | <1016 | Ω.m | |
電容率 | 60Hz | --- | 2.91 | --- | |
電容率 | 1MHz | --- | 2.85 | --- | |
介質(zhì)衰耗因數(shù) | 60Hz | --- | 6.6×10-4 | --- | |
介質(zhì)衰耗因數(shù) | 1MHz | --- | 9.2×10-4 | --- | |
耐電弧性 | --- | --- | 110 | sec | |
加工性能 | 成型收縮率 | --- | --- | 0.5~0.7% | % |
熱 性 能 | 線膨脹系數(shù) | --- | --- | 6.5 | ×10-5cm/cm/℃ |
燃燒性 | 3mm | --- | V-0 | --- | |
載荷撓曲溫度 | --- | --- | 148 | ℃ | |
維卡軟化點(diǎn) | --- | --- | 148 | ℃ |